I have a small project going on and am getting conflicting information about stringer layup schedule.
Background:
Hull is a 14 foot Ray Hunt designed hull built by O'Day in the early 60's.
.
I have stripped it down to the bare hull, lots of grinding to remove the majority of the stringer tabbing, etc.
New transom is in 3/4" Coosa across the entire transom and a double layer in the middle there the outboard will be mounted. Between the two layers is a layer of 1708 and a layer of mat. Bonded to transom with a VE bonding compound. Using VE resin so far. Inner glass is two layers of 1708.
Stringers are 3/4" Coosa. They have been scribed to hull and will be held in place (off the hull bottom) with the jig shown below such that I can use the same VE bonding putty to hold them in place before tabbing. Each stringer has 2 layers of 1708 on each side.
That brings me to where I currently stand.
For the transom, I have been told that the coosa with original skin on outside and two layers of 1708 on the inside is MORE than enough for a 75ish HP outboard. I initially thought that I would put a 3 layer on, but if what I already is more than sufficient I would not.
For the stringers, my thought was tabbing with two layers of 1708 onto the hull of 4" and 6" then capping the stringers with some 4" Unidirectional tape that I have.
Am I on the correct path?
Thanks in advance.
Ian.
Background:
Hull is a 14 foot Ray Hunt designed hull built by O'Day in the early 60's.
.
I have stripped it down to the bare hull, lots of grinding to remove the majority of the stringer tabbing, etc.
New transom is in 3/4" Coosa across the entire transom and a double layer in the middle there the outboard will be mounted. Between the two layers is a layer of 1708 and a layer of mat. Bonded to transom with a VE bonding compound. Using VE resin so far. Inner glass is two layers of 1708.
Stringers are 3/4" Coosa. They have been scribed to hull and will be held in place (off the hull bottom) with the jig shown below such that I can use the same VE bonding putty to hold them in place before tabbing. Each stringer has 2 layers of 1708 on each side.
That brings me to where I currently stand.
For the transom, I have been told that the coosa with original skin on outside and two layers of 1708 on the inside is MORE than enough for a 75ish HP outboard. I initially thought that I would put a 3 layer on, but if what I already is more than sufficient I would not.
For the stringers, my thought was tabbing with two layers of 1708 onto the hull of 4" and 6" then capping the stringers with some 4" Unidirectional tape that I have.
Am I on the correct path?
Thanks in advance.