Is this still available? If so, how old is it , what model is it, and how much are you asking. Also, where are you located? Thanks, Teresa. My...
How old is your system and how much are you asking? My email is teresapay@yahoo.com or you can call 419-289-9739. Thanks.
No release agent needed, just apply in circular motions and let dry 20-30 min, if you are concerned about residue on the mold, apply 2 THIN coats....
if you will be removing covers, be sure to add UV-9 inhibitor to your resin...
laminate thickness will be contingent on weight of glass fiber used, we use 1 1/2 oz CSM and you need 3 layers for each 1/8" of laminate thickness...
We have used Johnson paste wax as a mold release for 24 years...works great!
If you are going to have any fiberglass layup come in contact with it you will need a polyisocyanurate as styrene attacks others...
Call Scott Pay, he has 24 years experience, located in Ohio but may be able to work something out with shipping the part - 419-289-9739 or...
We have a guy that knows Venus/Magnum systems inside out and stocks parts as well as he can provide you with schematics, his name is Reed Schibley...