Hi Folks We use Plexus for gluing all Stainless & Ali to GRP Darren
Gell Coat is absolutley fine. Ensure you mix in 2% Wax Solution proir to adding the catalyst Ensure you abrade the area you intend to cover with...
There is a new transducer available that looks through the grp hull, therefore no drilling required We have just started using them in a large...
Hi We use 1152 PA (Filleting Paste) with a 50mm rad & then bond the bulkheads to the hull/deck using chop strand/biaxial/chop strand We use this...
We use Sika for many applications, some would be relevant Run this past the sika boys Abrade the ally and then apply sika primer prior to any...
They also make MA320 (I think thats the number) which has a working time of about 20 mins. They also make a Low Odour variant which is much...
Hiya George Sorry but I've never heard of it but we have had a lot of trouble using everything except balsa We have had to flatten back and...
Hiya Did you use a "plastic/foam core instead of basla.......
Hiya Hope the following helps 1) To maintain a certain thickness (ie so that the deck doesn't push all the plexus out) you can glue some...
By the number MA820 I suppose this is made by Plexus. We tend to use a large amount of this, please confirm & I will answer any questions that I...
Hi I have 14 years experience in the Boat Building buisness. For the past 6 years I have been managing a production Line of 94ft, 95ft, 100ft &...