Acmc Hey, just came across you thread. I would serious consider the Advanced Composites Manufacturing Centre ACMC - Its part of the university...
guide coat / dye After just reviewing our gelcoat repair procedure, its imparitive to match the sanding system to your gelcoat. i.e. a soft...
Hi, Having an electrical or water system imbedded close to the mould gelcoat surface is a great idea. However we need a failsafe system. What...
good idea but not practical Firstly, I forgot to mention, we also lag the inside of the hull with an ultra light weight, but highly thermo...
as hot as practically possible Hi, Before I get this topic going, this is the basis for dicussion. Current production is based around...
Just wondering who in the industry post cure very large laminates whilst still in the mould? By large, I thinking between 40-100ft structures...
mexicans are a very cheap labour source.
the quickest method of fairing is to use the longest board possible. But that depends on the wavelength of the deviation of ripples and labour....
Hi, You will be pleased to hear, your detailer is talking complete B*******s. Asuumption: repair is hand lamination only. The reason why a...
prevention better than cure I think theres a lesson to be learned with all no slip surfaces. Prevention to durt, grit and grim, in addition to...
infuse the moulding Hi, If you spending 5k on materials, it isnt going to cost not much to infuse the moulding. I'm sure someone across the...
If you were to take a splash off a good section of your non-slip, and form a basic mould from that, you can then lay up a single skin of non slip...
mould release system Hi, We have used chemlease for many years, and the system is a very reliable system provided moulds are maintained, treated...
Im a believer everything is repairable someone the question is at what cost? If that was my baby, I would repair from both sizes (inside and...