    Is the blush as prevalent using west system and microlite thickener?
    I have some glue lines that are concave and require extra filler. I dont want to scrub because of raw timber;Will a lite "edge folded" hand sand surfice?
     
  2. fiberglass jack
    Joined: Dec 2005
    Posts: 463
    Likes: 16, Points: 0, Legacy Rep: 95
    Location: toronto

    fiberglass jack Senior Member

    thats what i would do
     
  3. JR-Shine
    Joined: May 2004
    Posts: 341
    Likes: 4, Points: 18, Legacy Rep: 54
    Location: Vero Beach, FL

    JR-Shine SHINE

    You want to wipe it down, then sand, then wipe again. If you sand then wipe, you might just be grinding the blush into the surface.

    Joel
     
  4. Roly
    Joined: Jul 2005
    Posts: 508
    Likes: 23, Points: 18, Legacy Rep: 222
    Location: NZ

    Roly Senior Member

    Yep, I agree,but I don't want to wet the bare timber. Winter is coming on
    and the timber will be starting to absorb moisture. I will heater the hull inside
    prior to glassing. (In a couple of weeks. :))

    Just a thought, but what about giving a vigourous wipe around with a epoxy
    wet brush to take up the amine blush and redistribute it into the next mix?
     