    316 Ss

    316 stainless will NOT be magnetic. Lots of stainless steel is sold as 316, but the nickel, chrome, and molybendum mix actually used is a much...
    Post by: Shipwrighttech, May 27, 2014 in forum: Materials
  2. Shipwrighttech
    Post

    Anyone use polyaspartic coatings?

    Alexseal has a waterborne interior urethane that can be applied directly to wood/fiberglass/clean, sanded resin. Ventilate the engine room as...
    Post by: Shipwrighttech, May 27, 2014 in forum: Materials
  3. Shipwrighttech
    Post

    Please Help With Paint Questions

    OceanNavigator2, some of the larger concerns regarding use of industrial products in the marine environment are flexural properties, intracoat...
    Post by: Shipwrighttech, May 27, 2014 in forum: Materials
  • Find all content by Shipwrighttech
  • Find all threads by Shipwrighttech
  • Forgot your password?
Boat Design Net
Home Shipwrighttech >
Boat Design Net
Boat Design Net - the Boat Design and Boatbuilding Site connecting Boatbuilders and Designers on the Net
  • Home
  • Boat Design Forums

    Boat Design Forums

    Quick Links
    • Search Forums
    • Recent Posts
  • Boat Design Directory
  • Boat Design Gallery

    Boat Design Gallery

    Quick Links
    • Search Gallery
    • New Gallery Images
  • Bookstore
  • Thanks to our Site Sponsors
  • Menu
Search
More...
Style
Default Style
  • Boat Design Net
  • Forums
  • Gallery
  • Directory
  • Books
  • Powerboat Ads
  • Sailboat Ads
  • Contact Us
  • Help
  • Top
  • RSS
  • Terms of Use - Legal
  • Forum Rules
  • Privacy Statement
  • Cookie Statement
Forum software by XenForo™ ©2010-2017 XenForo Ltd. Web Site Design and Content Copyright ©1999-2026 Boat Design Net