Thanks Ondarvr, I also agree about the under curing. I am meeting supplies soon to fine the correct catalyst.
Spray single coat, brush on extra to corner ETC that may need further sanding. Haven't had any issues with adhesion thus far.
I think you may be on to something regarding reduced vacuum. Its something I am looking further into.
Foam is grooved and perforated. I dont think it is air being trapped, can't hear any air gap when tapping on the part. Infusing in two stages is...
Hi there, Yes, I think dimpling maybe wrong term, a wavey finish is more accurate. It doesn't look like pre-release. I will attempt to measurse...
Edit: We back the gelcoat up dry not wet.
Hi All, I'm an engineer at a company where we produce offroad expedition vehicles. We are vacuum infusing our fibreglass parts, but we are having...