Correct. The 200/500 are compounds to bring up a good surface finish. That will then be polished/ buffed up. So now as I understand it. I...
I really thought I would get an answer here. Forget it. its obviously beyond you to give a straight answer. This crap is not that hard. Its not my...
So the mould is primed and wet dryed to 1000. I now put on a flow coat high...
http://www.mbfg.co.uk/chemtrend-chem...ase-agent.html Has any one tried this gear
Yes I have had a look and thought it was great but, I need to spend more time reading. I am not just to sure of what he used to get a shine before...
Hello all from Scotland. We made a plug from an old salmon clinker coble. we then made a mould from the plug. Then we realized we had made a...