    Could I use the bondo hair for fileting?
     
  2. AnthonyW
    Joined: Oct 2012
    Posts: 115
    Likes: 10, Points: 18, Legacy Rep: 19
    Location: Cape Town, South Africa

    AnthonyW Senior Member

    Don't know about that - but I used cake flour - worked very well. Much easier than silica to sand and use (and fine sawdust is hard to get in my part of the world.)
     
  3. midcap
    Joined: Oct 2013
    Posts: 60
    Likes: 0, Points: 6, Legacy Rep: 10
    Location: United States

    midcap Junior Member

    hmm, I never thought about that.
     
  4. michael pierzga
    Joined: Dec 2008
    Posts: 4,862
    Likes: 116, Points: 0, Legacy Rep: 1180
    Location: spain

    michael pierzga Senior Member

    Wood dust.......clean out your vacume dust extractor
     
  5. midcap
    Joined: Oct 2013
    Posts: 60
    Likes: 0, Points: 6, Legacy Rep: 10
    Location: United States

    midcap Junior Member

    I'm trying to get something that is already mixed together though.
     
  6. michael pierzga
    Joined: Dec 2008
    Posts: 4,862
    Likes: 116, Points: 0, Legacy Rep: 1180
    Location: spain

    michael pierzga Senior Member

    Hmmmmmm

    Bondo is pretty crappy fillet material. Guess its better than bubble gum.

    Go for the fiber bondo.....precoat the substrate with resin first.

    Dont sail around the world with it.


    Hmmmm
     
  7. midcap
    Joined: Oct 2013
    Posts: 60
    Likes: 0, Points: 6, Legacy Rep: 10
    Location: United States

    midcap Junior Member

    I just noticed that I have some micro baloons on hand. That should work good.
     
  8. hoytedow
    Joined: Sep 2009
    Posts: 5,857
    Likes: 400, Points: 93, Legacy Rep: 2489
    Location: Control Group

    hoytedow Carbon Based Life Form

    I save the dust from my sander in plastic jars.
     
  9. michael pierzga
    Joined: Dec 2008
    Posts: 4,862
    Likes: 116, Points: 0, Legacy Rep: 1180
    Location: spain

    michael pierzga Senior Member

    Oh.....so you do have resin you just need filler...fibers are stronger than ballons
     
  10. midcap
    Joined: Oct 2013
    Posts: 60
    Likes: 0, Points: 6, Legacy Rep: 10
    Location: United States

    midcap Junior Member

    yep I have 10 gallons on hand. I don't think I would be able to get the fibers by tomorrow though. I just need the balloons to make a radius for me so the roven lays down better in the corner.
     
  11. michael pierzga
    Joined: Dec 2008
    Posts: 4,862
    Likes: 116, Points: 0, Legacy Rep: 1180
    Location: spain

    michael pierzga Senior Member

    Guess ya gotta do what ya gotta do.
     
  12. Milehog
    Joined: Aug 2006
    Posts: 571
    Likes: 121, Points: 43, Legacy Rep: 215
    Location: NW

    Milehog Clever Quip

    Some use talc.
     
  13. upchurchmr
    Joined: Feb 2011
    Posts: 3,287
    Likes: 259, Points: 83, Legacy Rep: 579
    Location: Ft. Worth, Tx, USA

    upchurchmr Senior Member

    Don't use saw dust, too coarse and it just balls up and won't smooth out.
    Sanding dust is perfect.
    Microballons are almost as good, a little sanding dust mixed in will provide a little desirable strength.

    Don't stop
     
  14. PAR
    Joined: Nov 2003
    Posts: 19,126
    Likes: 498, Points: 93, Legacy Rep: 3967
    Location: Eustis, FL

    PAR Yacht Designer/Builder

    It depends on what the fillet is. There are three primary fillet types, cosmetic, light and heavy structural. A cosmetic fillet is just as it sounds and doesn't need to have much more than the ability to hold it's shape when cured. These are used to clean up inside corners on a cockpit sole for easy washout (for example).

    A light structural fillet might or might not have a fabric over it, but it will be made of a structural filler material(s), such as silica, milled fibers, wood flour, cotton flock, etc. The filler materials often has something to do, such as increase bonding, compressive or tensile strength, etc. For example milled fibers is much preferred when bonding to 'glass.

    A heavy structural fillet is always covered with fabric, usually biax, though if the boat's small, regular cloth can be used. The filler materials are about the same as a light structural fillet, with emphases fibrous materials that have strength, stiffness and substrate bond effectiveness.

    Baby powder is an effective filler to help smooth out a fillet and makes sanding easier, but offer not real strength. corn, wheat or rice flour (yep, steal it out of her kitchen) is a good medium strength filler. Balloons and micro spheres have not strength, but do ease sanding effort and weight.
     

  15. midcap
    Joined: Oct 2013
    Posts: 60
    Likes: 0, Points: 6, Legacy Rep: 10
    Location: United States

    midcap Junior Member

    don't stop?
     
Loading...
Similar Threads
  1. Aziz THRAYA
    Replies:
    0
    Views:
    149
  2. Thule
    Replies:
    30
    Views:
    3,556
  3. NC.Traveler
    Replies:
    0
    Views:
    758
  4. AquaticFrank
    Replies:
    7
    Views:
    1,433
  5. Eric Lundy
    Replies:
    1
    Views:
    1,149
  6. Mark Rush
    Replies:
    7
    Views:
    1,713
  7. Swamp_Yankee
    Replies:
    16
    Views:
    3,144
  8. ArthurFusco
    Replies:
    9
    Views:
    1,725
  9. loneranger
    Replies:
    7
    Views:
    1,838
  10. Reid Crownover
    Replies:
    8
    Views:
    1,911
Forum posts represent the experience, opinion, and view of individual users. Boat Design Net does not necessarily endorse nor share the view of each individual post.
When making potentially dangerous or financial decisions, always employ and consult appropriate professionals. Your circumstances or experience may be different.