OK, after i upload some pics on flickr. I will send you the pics links. I am a camera fan too. Nowadays, we can use cellphone camera to record...
We have ripped off the plug with mold gel coat. The surface is terrible. You can give your email address, and i will send you some pics of it.
We just used paste wax,meguair, 9 times waxing. It is the mixing spray killed me. The porosity of EZ sanding stucked the mold. When we pull off...
Yes, wax applying is the same, the only variation is mixed spraying. Thank you Jeff.
Somehow, workers mixed duratec EZ sanding and high gloss coating together on plug to save one time spraying. Then we end up with a stuck mold. The...
:D:D I am here all the time. Never heard of coosa from my suppliers. Sounds like a good choice for structure.
COOSA,PENSKE? What is it? Never heard.
There is an interesting article on West system website. You might get your answer from it. http://www.westsystem.com/ss/thinning-west-system-epoxy/
Ma also can mean scold~~:D:D
There is not only certificate on DNV site, it has boat design and building standard too.
You can find your answer in the DNV related rules.
Wow, i didn't receive the private mail from you about you are coming to my company. :D:D Terrific.
Thanks,MM. Shiny problem is from wax.I found the Meguiar wax here is from a trader with very cheap price, the trader must blend in some impurity....
Thanks for all your guy's replies. The truth is we do clean the wax we apply on the mould, use clean cloth to wipe it off. Picture won't show us...
There are some types of small boat here in my working place,like 17ft,19ft. The profits of these boats is too low, sometimes just enough for...
The plan is making the best mold, :D:D:D, disregarding cost, and my boss trust the project director because of the money earning plan he describes.
We are building a boat floating on the ocean, not a missile or F35 which requires very high dimensionally accuracy parts, those molds should be...
I don't know. We also use Zero shrinkage tooling resin here,Nord2000 or 3000. It is for glass fiber mold. Somehow carbon fiber has to match up...
Yeah, I just persuade the project director to infuse the mold. We threw away one big carbon fiber mold a week ago, just for massive void on WR300.
hahahaha~~Funny one,:D:D:D:D. CSM is short for Chopped strand mat.