Polyesters are chemically unstable. They will to varying degrees (speed) all hydrolyse ie break down. Probably not in your life time (but that...
All epoxies will absorb small amounts of moisture and as someone said it diffuses in...and out all the time when it reaches saturation point....
Hey Tony I imagine if you have been spraying Imron, then you won't find Alexseal a problem. It is better to spray Alexseal slightly thicker every...
Ps a lot of the us Alexseal guys are ex awlgrip. They are great help.
Alexseal is used by many big builders in Europe with good results. It sprays different than awlgrip but a good painter will get good result. Thin...
I'd gusee you never studied Chemistry to a high level. if you gave me time I could probably rack my brains to work out how much o2 you would need...
Has the boat been covered with a tarpaulin? This can cause this. You say the boat is in Holland...which implies it has travelled...which does...
Just paint the whole deck area with your spec'd system. Mark of your non-skid areas. Roll these. In Holland we roll De Ijssel which rolls great,...
what he said. We wet sand loads. We wash down as we go with sponge. The crap that goes back in to bucket will be pretty settled overnight. If...
http://www.moldedfiberglass.com/sites/default/files/docs/MFG_Technical_Design_Guide_FRP_Composite_0.pdf google is pretty handy:)
loads of uk builders use durabuild. You can use a good 2 pack polyurethane. In Holland deijssel is used but you can use International...
What he said. The standard length is approx. 1.8m or something. Cut it to about 80cm. Buy sturdy clips like you get on clip boards and screw...
What primer do you have? I am only asking as you mentioned filler. Some alumigrip primers are for aluminium but in different situations. ie no...
Ideally blast the alu with appropriate grit media...failing that disc it with p24 on angle grinder. If you use a big grinder you will do area in...
Steve You are right to be wary of all claims. My beef with the comments here were the black/white comment that interprotect 2000e was not a...
We will leave it here. You are right, the permeability of Interprotect 2000e is not very good. It is a good barrier. I wasn´t proposing use as...
Actually interprotect is almost 100% solid WHEN it is cured...ie once the solvent evaporates:) Unlike most 100%solid epoxies which are loaded with...
Sorry if I confused topic by being less than precise talking about Interprotect 2000e. The OP mentioned this, I was talking of this. I must...
what bit don't you guys understand? Interprotect isn't the barrier????? No. NO NOO. Epoxy is the resin you use to seal the open...