#1
| |||
| |||
| West sys. glue mix Is the blush as prevalent using west system and microlite thickener? I have some glue lines that are concave and require extra filler. I dont want to scrub because of raw timber;Will a lite "edge folded" hand sand surfice? |
|
#2
| |||
| |||
| thats what i would do |
|
#3
| |||
| |||
| You want to wipe it down, then sand, then wipe again. If you sand then wipe, you might just be grinding the blush into the surface. Joel |
|
#4
| |||
| |||
| Yep, I agree,but I don't want to wet the bare timber. Winter is coming on and the timber will be starting to absorb moisture. I will heater the hull inside prior to glassing. (In a couple of weeks. )Just a thought, but what about giving a vigourous wipe around with a epoxy wet brush to take up the amine blush and redistribute it into the next mix? |
![]() |
| Thread Tools | Search this Thread |
| Display Modes | |
| |
Similar Threads | ||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Looking for molds on the west coast 22-28 | COLE | Boat Molds | 3 | 04-18-2007 12:21 PM |
| oil mix for johnson hydro electric V115? | revshot | Propulsion | 0 | 02-10-2006 01:29 PM |
| Kerosene Mix With Diesel | PADDLEGUY | Open Discussion: All Things Boats & Boating | 15 | 02-06-2006 03:29 AM |
| Sit - mix a drink - sail fast... | Sean Herron | Boat Design | 5 | 03-14-2005 10:44 AM |
| Placed to buy mix and pour foam | jtdouglas3 | Fiberglass and Composite Boat Building | 3 | 10-01-2004 05:23 PM |